corrosion test![]()
Valve detection![]()
Metallographic analysis![]()
component analysis![]()
Mechanical test![]()
failure analysis![]()
Nondestructive flaw detection![]()
2017-02-27 Rongda test 1043 times
Detection Purpose: Stress corrosion of metal in static high temperature water
Detection range: Stainless steel, iron - nickel - based alloy, nickel - based alloy and other iron - chromium - nicke
High temperature water stress corrosion test:
Corrosion damage caused by a combination of residual or applied stress and corrosion.
Crack initiation time:
The time between the beginning of the test and a crack being detected by some means.
Rupture time:
The time elapsed from the beginning of the test to the rupture. The criterion of fracture is: the crack appears first; Sample separation as a whole; An agreed middle ground.